Industrielle Nutzung: | Lebensmittel |
---|---|
Transparenz: | Transparent |
Layered: | Basisstufe |
Härte: | Weich |
Grundstufe: | BOPP |
Heat Seal: | LDPE |
Lieferanten mit verifizierten Geschäftslizenzen
Eigenschaften | Testmethode | Einheit | Typischer Wert | ||||
Dicke | Kincess | μm | 12 | 15 | 18 | 20 | |
Dickenvariation | Astm-252-78 | % | ±4,0 | ±3,5 | ±3,0 | ±3,0 | |
Ertrag | Kincess | m2/kg | 91,6 | 73,3 | 61,1 | 55,0 | |
Zugfestigkeit | MD | ASTM D-882 | Mpa | 150 | 150 | 155 | 160 |
TD | ASTM D-882 | Mpa | 280 | 280 | 280 | 280 | |
Dehnung Beim Bruch | MD | ASTM D-882 | % | 160 | 160 | 160 | 160 |
TD | ASTM D-882 | % | 60 | 60 | 60 | 60 | |
Reibungskoeffizient | T/T-US | ASTM D-1894 | - | 0,25 | 0,25 | 0,25 | 0,25 |
T/O-US | ASTM D-1894 | - | 0,30 | 0,30 | 0,30 | 0,30 | |
Wärmeschrumpfung | MD | ASTM D-1204 | % | 4,0 | 4,0 | 4,0 | 4,0 |
TD | ASTM D-1204 | % | 1,5 | 1,5 | 1,5 | 1,5 | |
Dunst | ASTM D-1003 | % | 1,2 | 1,2 | 1,2 | 1,2 | |
Glanz | ASTM D-2457 | - | 92 | 92 | 92 | 92 | |
Netzspannung | ASTM D-2578 | Dyn | 38 | 38 | 38 | 38 |
Lieferanten mit verifizierten Geschäftslizenzen